DigiTan said:Eh, don't worry about it. So far, I've been pre-cleaning the iron tip with rubbing alcohol and its advertised at 40W. The flux/earwax is Kester Rosin Paste Flux "formula SP-44." One of the key ingrediants is petroleum jelly. I applied with a dental tool, also pre-cleaned with alcohol. :?
I presume your iron ISN'T temperature controlled?, it would be a LOT better if it was. I'm also bemused by cleaning the bit with rubbing alcohol?, there seems no need (or use?) in such a procedure. Just tin the bit, and wipe it on a damp sponge.
But what you do need is liquid flux, not the paste type - it makes a massive difference to SM soldering.
And WHATEVER you do, DON'T attempt to glue the parts down :lol: